PROBLEM TO BE SOLVED: To provide a thermoplastic resin composition that becomes a molded article having high toughness even if the addition amount is very small without impairing the basic physical properties of the thermoplastic resin, and heat obtained by the thermoplastic resin composition Provision of plastic resin moldings. A thermoplastic resin in which the content of at least one of a saccharide compound alone, a saccharide compound and a polyhydric phenol compound is 0.002 parts by mass to 1.5 parts by mass with respect to 100 parts by mass of the thermoplastic resin. It is a composition, and the saccharide compound includes a monosaccharide, a disaccharide, an oligosaccharide, and a polysaccharide, and the polyhydric phenol compound includes a tannin compound. [Selection] Figure 1 |