Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_4edd4e526605dbd18b513b4b30d19ab2 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-0585 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-054 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-587 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-133 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-05 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-054 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-0569 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-0568 |
filingDate |
2005-02-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d2816fd52139c1d03ee1b804c99e4fdc http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0a7c6d8deca6effb7caef56caaa12939 |
publicationDate |
2006-08-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2006216511-A |
titleOfInvention |
Nonaqueous electrolyte secondary battery |
abstract |
PROBLEM TO BE SOLVED: To provide an inexpensive non-aqueous electrolyte secondary battery capable of reversible charging / discharging. SOLUTION: A negative electrode active material containing carbon capable of occluding and releasing potassium and polyvinylidene fluoride as a binder are added and mixed to prepare a slurry as a negative electrode mixture. Examples of carbon contained in the negative electrode active material include graphite. Next, a slurry is prepared by adding N-methyl-2-pyrrolidone to the negative electrode mixture and kneading. Subsequently, a negative electrode is produced by apply | coating a slurry to a negative electrode electrical power collector. As the non-aqueous electrolyte, a non-aqueous solvent in which ethylene carbonate and diethyl carbonate are mixed at a volume ratio of 50:50, and potassium hexafluorophosphate as an electrolyte salt has a concentration of 0.7 mol / l. The one added as described above is used. [Selection] Figure 1 |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2016059907-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2016059907-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10593992-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2017510971-A |
priorityDate |
2005-02-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |