Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_14df928cce1112b89356928855b60351 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L101-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B1-04 |
filingDate |
2005-02-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6b224a0474d43d6b2a887fe26de6d6b7 |
publicationDate |
2006-08-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2006213759-A |
titleOfInvention |
Optical material and optical element |
abstract |
An optical stability is reliably increased. An optical material includes a thermoplastic resin, inorganic particles, and at least one additive of an antioxidant and a light-resistant stabilizer, and the content G 1 of the additive is G 0 > G 1. > S 1 (where G 0 is the content of the inorganic particles and S 1 is the saturated dissolution amount of the additive in the thermoplastic resin). [Selection] Figure 1 |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2011090341-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2009057398-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8854733-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2013011663-A1 |
priorityDate |
2005-02-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |