http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2006169699-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_5d123e76a98aad8db100e9f8c62e0648 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F6-92 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F6-62 |
filingDate | 2004-12-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1d2f92e8c3f252ff23c68da06e9e6cdf http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8c0ac0bd84f714539d83fe509548ee11 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b1f7cdc86b030f2688ed9fb2b3f89897 |
publicationDate | 2006-06-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2006169699-A |
titleOfInvention | Polyester fiber |
abstract | An object of the present invention is to provide a polyester fiber which is excellent in hue, can be produced industrially, and has a very small amount of foreign matter generated even when melt-spun continuously through a spinneret for a long time, and which is stably spun at high speed. The content of a metal element having a specific gravity of 5.0 or more is 0 to 10 ppm by weight, the crystal size L (Å), the birefringence of the whole fiber (ΔN), and the birefringence of an amorphous region ( (DELTA) Na) The polyester fiber which satisfies the requirements of following (1)-(3). (1) 0.08 ≦ ΔN ≦ 0.12 (2) 0.05 ≦ ΔNa / ΔN ≦ 0.75 (3) 300 ≦ L / ΔN ≦ 700 [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2010111961-A |
priorityDate | 2004-12-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 77.