http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2006152058-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_ce3959dcd88bcf905c8e00887549ac33 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L31-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L9-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L7-00 |
filingDate | 2004-11-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d71271b574aa778632e346f642853506 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5f2e875f5e7d1b166c001c180b9973a5 |
publicationDate | 2006-06-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2006152058-A |
titleOfInvention | Rubber composition |
abstract | PROBLEM TO BE SOLVED: To provide a rubber composition containing a rubber component composed of natural rubber and / or a diene synthetic rubber, and particularly capable of obtaining a lightweight vulcanized rubber having a low density after vulcanization. provide. SOLUTION: With respect to 100 parts by weight of a rubber component composed of natural rubber and / or diene synthetic rubber, closed cells having a foaming density of 0.03 to 0.40 g / cm 3 and a particle size of 5 mm or less are provided. A rubber composition containing 10 to 100 parts by weight of the incorporated ethylene-vinyl acetate copolymer foam and having a density after vulcanization of 0.85 to 1.20 g / cm 3 is obtained. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-109233013-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-5568698-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-109233013-B http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2015019490-A1 |
priorityDate | 2004-11-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 42.