Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_129e393582e6bdf4029baf2206522f45 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02W30-82 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02W30-78 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02W30-62 |
classificationIPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L101-16 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B09B5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B09B3-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A63F7-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L97-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L67-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L59-00 |
filingDate |
2004-11-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_635ab01ec7364706e6d4e721d86c5fd8 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1101efe40e5440cf9324309bff3aea28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f481232ec331480cdfbba6fb39c27963 |
publicationDate |
2006-06-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2006152048-A |
titleOfInvention |
Recycled molding material and method for producing the same |
abstract |
【Task】 It is possible to protect the environment by reducing the amount of waste and reducing the use of petroleum resources, and at the same time provide recycled materials with excellent strength efficiently and inexpensively. In particular, to provide a reclaimed molding material and a manufacturing method that can greatly contribute to the reduction of the amount of waste of gaming machines. [Solution] The present invention includes a recovered material containing natural fibers and / or a wood-based material and an unused polylactic acid resin, and the mixing ratio of the recovered material with respect to the total weight is in the range of 15 to 85% by weight. It is the characteristic recycled molding material. [Selection figure] None |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2018518557-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008011946-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2015052876-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2009103812-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2008102747-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-104877319-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-7232102-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008201830-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008222856-A |
priorityDate |
2004-11-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |