http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2006116652-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c46533e1bf04b5107543aa61c06dc5e5 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09K3-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B24B37-00 |
filingDate | 2004-10-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ac04d09350f30614409e7f9f9239f262 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d1202d7231aa8a2cb93e32e3e7f5c1b3 |
publicationDate | 2006-05-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2006116652-A |
titleOfInvention | Polishing method and polishing body |
abstract | PROBLEM TO BE SOLVED: To provide a polishing method capable of forming a regular processed surface without limiting the shape or material of an object to be polished if it is non-magnetic and good in terms of cost even in a small amount and a variety, and obtained by the method An abrasive body is provided. A polishing method using a magnetic polishing fluid 1 containing magnetic particles, polishing particles and a medium, wherein the magnetic polishing fluid 1 is disposed on one surface of an object 2 to be polished, and the other A polishing method in which a magnetic pole 3 is disposed outwardly on a surface, and the magnetic polishing fluid 1 is thickened by generating a magnetic field in the magnetic pole, and the object to be polished is moved. [Selection] Figure 1 |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-114378675-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2014083647-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/TW-I637811-B |
priorityDate | 2004-10-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links