http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2006111873-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_ad2cd796f8c4dcb425ddcc68707d3444 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L63-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-36 |
filingDate | 2005-09-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_242090161c33efe449075ed6b5bcc72b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_330a0c8ee687e305fcb370dfffeadf60 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ed339e882a8b01fd21bb925ec9148924 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f5eb4b241e0e8640066b0703ad43d24c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5553bb1e61d933eb8d111854b0671b99 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b5b9360ddd4740ae6f8dc6d3a8c36d43 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8f8a6ab5c06f685ef0eb1fc4352a32a6 |
publicationDate | 2006-04-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2006111873-A |
titleOfInvention | Polyester composition and polyester molded body comprising the same |
abstract | PROBLEM TO BE SOLVED: To provide a molded object such as a hollow molded article, a sheet-like article, a stretched film, etc. having excellent transparency and little fluctuation in transparency, and suppressing the production and fluctuation of aldehydes such as acetaldehyde during molding. Efficient production of high-speed molding of polyester compositions that are suitable for use as materials such as coatings, hollow molded products with excellent pressure resistance or heat-resistant dimensional stability, especially hollow molded products with excellent pressure resistance and heat and pressure resistance It is an object of the present invention to provide a polyester composition that can be produced and a polyester molded article comprising the same. A polyester composition comprising at least two polyesters having substantially the same composition as a main component, wherein the difference in intrinsic viscosity of the polyester is in the range of 0.05 to 0.30 deciliter / gram. The polyester composition is characterized in that the difference in crystallization temperature when the polyester is heated is within 15 ° C., and the difference in crystallization temperature when the polyester is lowered is within 20 ° C. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-2180017-A2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2017203116-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8445785-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8410208-B2 |
priorityDate | 2004-09-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 265.