Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1d29f7ac2c7f9be9f7dae1a83bbb5c92 |
classificationIPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B103-12 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B28-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B22-10 |
filingDate |
2004-10-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4d7ad714fdd5cca082daf2d870909dca http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_585d3503f7d6fb69f57a140ae2c58c5c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_83c67f78f8bf3da4277cf4a0bd543c97 |
publicationDate |
2006-04-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2006111485-A |
titleOfInvention |
Setting accelerator for cement and cement composition |
abstract |
PROBLEM TO BE SOLVED: To provide a setting accelerator having an excellent setting acceleration effect and a cement composition using the setting accelerator without causing a phenomenon that adversely affects the durability of a cured body such as corrosion of reinforcing bars or alkali aggregate reaction. provide. SOLUTION: An agglomeration accelerator for cement comprising calcium carbonate adjusted to an average particle size of less than 0.7 μm, preferably 0.05 to 0.6 μm, and the agglomeration accelerator is added in an amount of 0. It is a cement composition containing 1 part by mass or more and less than 10 parts by mass. [Selection figure] None |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-109923088-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-4688657-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2018087099-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-109923088-B http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2007153683-A |
priorityDate |
2004-10-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |