http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2006104370-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_56abb7a905b2aba4c53d3d3debee8c14 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G63-605 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G63-065 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G63-78 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G63-19 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K19-46 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-19 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L67-03 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-04 |
filingDate | 2004-10-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_babe6a79508bd8d974f78a25acf61cc8 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d36fa9ff85a2208cb7e5b60455a0255d |
publicationDate | 2006-04-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2006104370-A |
titleOfInvention | Method for producing wholly aromatic liquid crystal polyester resin |
abstract | PROBLEM TO BE SOLVED: To provide a method for producing a wholly aromatic liquid crystal polyester resin excellent in color tone, thermal stability and mechanical properties, a liquid crystal polyester resin obtained by the method, and a liquid crystal polyester resin composition containing such a liquid crystal polyester resin. [MEANS FOR SOLVING PROBLEMS] 1) Hydroxyl group of one or more main monomers selected from aromatic hydroxycarboxylic acids, aromatic diols and aromatic dicarboxylic acids, which essentially contain aromatic hydroxycarboxylic acids and / or aromatic diols Acylating with an acylating agent; and 2) a step of polycondensing the main monomer whose hydroxyl group is acylated, And a method for producing a wholly aromatic liquid crystal polyester resin, wherein the polycondensation reaction step is performed in the presence of 1 to 5000 ppm of metal dihydrogen phosphate with respect to the weight of the total monomer, and the liquid crystal polyester resin is included. A liquid crystal polyester resin composition is provided. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2014506952-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2013170202-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2016060872-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2010126231-A3 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2013543911-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101927993-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9029496-B2 |
priorityDate | 2004-10-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 142.