Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_669c01133740c5233f2c8738904ea3af |
classificationIPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29K23-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29L7-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29K105-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29L9-00 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C48-305 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C47-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/E04F13-07 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C47-04 |
filingDate |
2004-09-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a3fac4facd27ab3c7796b0971e9f6157 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_99bb8fe9d975b3b0191bb7e8a2e2a51a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_615e9f0daee38e7ca5419e44e000ffe0 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8f3ca11b9e20cad1b2c2835b92e7b2ef http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b582cbda84300d4b28519fa4de04a807 |
publicationDate |
2006-04-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2006095986-A |
titleOfInvention |
Method for producing foam wallpaper |
abstract |
The present invention provides a method for producing a foam wallpaper having high productivity and a good foamed state. A composition for forming an unfoamed resin layer containing an ethylene-vinyl acetate copolymer resin and a thermally decomposable foaming agent is extruded on a paper base by a T-die extruder, so that it is not yet formed on the paper base. In the method for producing foamed wallpaper, after laminating the foamed resin layer, the resin layer is irradiated with an electron beam to crosslink the resin, and then the resin layer is heat treated to foam the pyrolytic foaming agent. (1) The melt flow rate of the composition at the time of T-die extrusion is 40 g / 10 min or more, (2) The production method characterized in that the melt flow rate of the unfoamed resin layer subjected to heat treatment is 20 g / 10 min or less. [Selection figure] None |