http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2006095971-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_14df928cce1112b89356928855b60351 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29K1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29L7-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02F1-13363 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02F1-1335 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B5-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C41-24 |
filingDate | 2004-09-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d99aee014a2b76b19a2c07168d061524 |
publicationDate | 2006-04-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2006095971-A |
titleOfInvention | Method for producing cellulose ester film |
abstract | PROBLEM TO BE SOLVED: To produce a cellulose ester film particularly useful for a protective film for a polarizing plate and a retardation film by a solution casting method, and depositing and accumulating calcium and magnesium compounds on the surface of a casting support Prevents the occurrence of adhered deposits (dirt). A high-quality cellulose ester film suitable as a protective film for polarizing plates is produced with extremely high productivity. After the cellulose ester dope is produced, the dope is cast on a support within 24 hours after the dope is brought to a temperature lower than the boiling point of the solvent by 5 ° C. or less. Within a range of 2 ° C. to 10 ° C. from the temperature of the support immediately after the web is peeled in the space near the support surface from the web peeling point of the endless support that moves indefinitely to the casting point where the dope is cast again. After supplying the wind controlled to a low water dew point and peeling the web from the support, the time until casting the dope on the support again is 1 to 5 seconds. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008201902-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008063403-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2017007261-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008207366-A |
priorityDate | 2004-09-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 114.