http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2006091272-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_03d0f52bb4069f8a19d70dcfb697c67a |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02F1-13363 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02F1-1335 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B5-30 |
filingDate | 2004-09-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_aa9ce8b6c94da38c483aefa66a8bf25f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_391b850040de2d082bda7fa4bbd4dc30 |
publicationDate | 2006-04-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2006091272-A |
titleOfInvention | Polarizing plate and liquid crystal display device using the same |
abstract | PROBLEM TO BE SOLVED: To provide a polarizing plate in which light leakage generated in a frame shape in a liquid crystal panel due to heat distortion or the like, and a liquid crystal display device having high display quality provided with the polarizing plate. SOLUTION: A polarizing plate having a layer structure in which an adhesive layer 1, an optical compensation sheet 2, a polarizing film 3, and a protective layer 4 are sequentially laminated, wherein the photoelastic coefficient of the adhesive layer is Cn (1 / Pa) and protection. When the film thickness of the layer is Tt (μm) and the elastic modulus of the protective layer is Et (Pa), the value Y1 of the following formula (1) or the value Y2 of the following formula (2) is 0.0006 or less. A board. Y1 = −700,000 × Cn + 0.075 / Tt−0.0002375 (1) Y2 = −700,000 × Cn + 3.56 × 10 6 /Et−0.0001762 (2) [Selection] Figure 3 |