http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2006052380-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c1755eede76ea7e719a3e0d2843cd793 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-17 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J11-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L63-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J163-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L101-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J201-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J133-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L33-14 |
filingDate | 2005-05-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e6c3d604d73e97dc42db7c5913a086c5 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_34bb3fc9d2c40f780c34eb72e3e64fd8 |
publicationDate | 2006-02-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2006052380-A |
titleOfInvention | Room temperature curable composition |
abstract | PROBLEM TO BE SOLVED: To provide a room temperature curable composition which reacts with moisture in the atmosphere at room temperature and cures in a rubbery shape, and has a low gloss after curing. SOLUTION: At least 0.5 silicon atom-containing groups that can be cross-linked by forming a siloxane bond are averaged per molecule, and a hydroxyl group or a hydrolyzable group is bonded to the silicon atom of the silicon atom-containing group. A room temperature curable composition comprising 100 parts by weight of an organic polymer and 0.1 to 10 parts by weight of a tertiary amine compound having a melting point of 20 to 60 ° C. [Selection figure] None |