http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2006051662-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_4ad033f38114362cc6d607044dbc8ff9 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L67-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-18 |
filingDate | 2004-08-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9eb7874b9577087526e5db6b308124e3 |
publicationDate | 2006-02-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2006051662-A |
titleOfInvention | Biaxially stretched polyester film |
abstract | PROBLEM TO BE SOLVED: To provide a film suitable as a constituent material for packaging materials such as industrial materials, pharmaceuticals, sanitary materials, foods, etc. having excellent film forming stability and good hand cutting properties. A film having a polyester layer (A layer) containing a butylene terephthalate unit and having a melting point of 240 ° C. or lower, wherein the end tear resistance value in the longitudinal direction of the film is smaller than the end row resistance value in the width direction. A biaxially stretched polyester film, wherein the end-row resistance in the longitudinal direction and the width direction is 40 N or less. [Selection figure] None |
priorityDate | 2004-08-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 41.