http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2006028383-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_f98e29df4b2d0cac7db5caa4ca887afa http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_d1a84d1b7b5e81f099ec2d4d905a74fc |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L91-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L99-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L53-02 |
filingDate | 2004-07-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4a713fcf0616178b2365b6c64464e270 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_cf064cfbebfc9caa703b1c107755eb0f |
publicationDate | 2006-02-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2006028383-A |
titleOfInvention | Dipping molding composition for polyurethane bonding and solvent paste |
abstract | PROBLEM TO BE SOLVED: To provide a dipping moldability composition for polyurethane adhesion and a solvent paste, which are particularly excellent in adhesion to polyurethane and excellent in flexibility and insulation. The present invention comprises an isobutylene block copolymer composed of an isobutylene compound block and an aromatic vinyl compound block, and at least (b) hydrogenated and / or partially hydrogenated copolymers 1 to 80 parts by weight, (c) a non-aromatic rubber softener 1-100 parts by weight, (d) a polyurethane dipping composition selectively containing 1-50 parts by weight of a petroleum resin, and this composition as a solvent A composition and a solvent paste obtained by dissolving in 80 to 400 parts by weight. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2010106403-A |
priorityDate | 2004-07-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 205.