http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2006026905-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_2d4d8115282cf75bb54e672fbbdb0576 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B41M5-502 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B41M5-52 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B41M5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B41M5-52 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B41M5-50 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B41J2-01 |
filingDate | 2004-07-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_869e8ded3db31337c7d28fde4ea20dc5 |
publicationDate | 2006-02-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2006026905-A |
titleOfInvention | Ink jet recording paper manufacturing method and ink jet recording paper |
abstract | PROBLEM TO BE SOLVED: To provide an ink jet recording paper manufacturing method with high color development, reduced ink absorption unevenness, suppressed white background contamination and stain during long-term storage, and ink jet recording paper manufactured thereby. provide. In a method for producing an ink jet recording paper, a coating liquid containing inorganic fine particles and a binder is coated on a support to form at least one porous ink receiving layer. Thereafter, a second coating solution having pH buffering properties is applied during the drying step, the pH of the porous ink-receiving layer coating solution is set to pH a , the pH of the second coating solution is set to pH b, and ink jet recording paper A method for producing an ink jet recording paper, wherein the conditions defined by the following formulas (1) and (2) are simultaneously satisfied when the pH of the film surface is pH c . Formula (1): pH b -pH c <1.0 <pH c -pH a , Formula (2): pH a <pH b [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2009202368-A |
priorityDate | 2004-07-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 62.