http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2006022340-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_6c8d4dc7bd1a30d8fda907fceaeb4e69 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B65D1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-183 |
filingDate | 2005-09-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6a8873276666038d3c3f15a5aa94015c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7b1c471c26002f0c0b7cac52d7813781 |
publicationDate | 2006-01-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2006022340-A |
titleOfInvention | Polyester resin |
abstract | [PROBLEMS] To achieve molding without reducing the transparency even if the molding temperature is lower than that of the conventional molding, so that generation of acetaldehyde during molding and mold contamination during molding are suppressed, and molding with excellent transparency is also achieved. It is possible to obtain a body, and particularly to provide a polyester resin suitable for forming a bottle for food and drink. A dicarboxylic acid component having terephthalic acid or an ester-forming derivative thereof as a main component and a diol component having ethylene glycol as a main component are produced by polycondensation through an esterification reaction or a transesterification reaction. Polyester resin, wherein the haze of a molded article injection-molded at 270 ° C. is 50% or less at a thickness of 5 mm. [Selection] Figure 1 |
priorityDate | 2005-09-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links