http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2006003751-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_be92719b856db86c092cc233e9512ca2 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G5-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G5-05 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G5-00 |
filingDate | 2004-06-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6845aa070f61e30b365cd9a0ecc28d00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_18cc64ca079ef945aa0d7eef61f69720 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_43b00aff439bc1bfb1172aadca45659b |
publicationDate | 2006-01-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2006003751-A |
titleOfInvention | Method for producing electrophotographic photosensitive belt |
abstract | PROBLEM TO BE SOLVED: To apply a coating solution using an organic solvent as a solvent to a plastic film whose surface is subjected to a conductive treatment, and to dry at a temperature of 110 ° C. or more for 10 minutes or more to form an electrophotographic photoreceptor layer. Even if the length is 2 m or more, the humidity is adjusted without occupying a large area, and an electrophotographic photosensitive member with extremely high dimensional accuracy is produced. A coating liquid containing an organic solvent as a solvent is applied once or a plurality of times to a plastic film having a thickness of 50 μm or more and 150 μm or less subjected to conductive treatment by aluminum vapor deposition or ITO vapor deposition. It is dried at the above temperature for 10 minutes or more to form an electrophotographic photosensitive layer having a film thickness of 15 μm or more, which is once cut into a size longer than the final dimension, and the same as the cut electrophotographic photosensitive sheet. An electrophotographic photosensitive film characterized by alternately stacking paper made of cellulose fibers having a thickness of 20 μm or more and 200 μm or less and allowing to stand for 9 hours or more, and then cutting the electrophotographic photosensitive sheet to a final dimension. Manufacturing method of body sheet. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2007213044-A |
priorityDate | 2004-06-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links