http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2006003389-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_03d0f52bb4069f8a19d70dcfb697c67a |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C1-498 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C1-74 |
filingDate | 2004-06-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7c66dbe9104107fcbb9fad1bd814e2cc |
publicationDate | 2006-01-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2006003389-A |
titleOfInvention | Method for producing photothermographic material and photothermographic material |
abstract | PROBLEM TO BE SOLVED: To provide a method for producing a photothermographic material having a small environmental pollution load and improved processing unevenness and graininess. An image forming layer coating solution containing a photosensitive silver halide, a non-photosensitive organic silver salt, a reducing agent and a binder, and a photothermographic material on which a non-photosensitive coating solution is coated and dried on a support. A method for producing a photothermographic material, wherein at least one of the coating solutions comprises a compound represented by the following general formula (E): R- (L) p -SO 3 M general formula (E) [In General Formula (E), R represents an alkyl group having 5 to 30 carbon atoms, and M represents an alkali metal ion or an ammonium ion. L represents a divalent linking group containing no aryl group or heterocyclic group. p is 0 or 1; ] [Selection figure] None |
priorityDate | 2004-06-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |