http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2006001884-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_95eaed79dec59391549e8016815b3a8f |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61Q1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61K8-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61K8-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61Q19-00 |
filingDate | 2004-06-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ce1ef72f8d51df07a863a05773e057fd http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_82c11a7989773ee73a699b0faf29a7b1 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_561eafa99c9fdb3968b77d57d43ed395 |
publicationDate | 2006-01-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2006001884-A |
titleOfInvention | Method for producing solid cosmetic |
abstract | PROBLEM TO BE SOLVED: To provide a method for producing a solid cosmetic material having a substantial funicular area. A method for producing a cosmetic comprising 1) 40 to 75% by mass of powder and 2) 20 to 50% by mass of an oily component having fluidity under the conditions of 1 atm and 25 ° C. There is provided a production method comprising a step of mixing a body and an oily component using an extrusion mixing device. In the cosmetic, the viscosity at 20 ° C. of a mixture of an oily component having fluidity under the conditions of 1 atm and 25 ° C. constituting the cosmetic and a component soluble in the oily component is 400 to 400 ° C. It is preferably 1000 millipascal seconds. [Selection figure] None |
priorityDate | 2004-06-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |