http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2005518460-A
Outgoing Links
Predicate | Object |
---|---|
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G64-42 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G64-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G64-307 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G64-30 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G64-30 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G64-42 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G64-14 |
filingDate | 2002-08-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2005-06-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2005518460-A |
titleOfInvention | Method for producing polycarbonate |
abstract | 【Task】 Providing polycarbonate with improved end-capping rate. [Solution] The polycarbonate having an improved end-capping rate is preferably produced by adding an end-blocking agent to the polycarbonate after the number average molecular weight of the polycarbonate reaches about 2000 to 15000 daltons. This endblocker has the following formula: [Chemical 1] Wherein R 1 is phenyl, phenoxy, benzyl, or benzyloxy, R 2 is C 1 -C 30 alkyl, C 1 -C 30 alkoxy, C 6 -C 30 aryl, C 6 -C 30 aryloxy, It is selected from C 7 -C 30 aralkyl, and C 7 -C 30 group consisting aralkyloxy. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2016020315-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2017047560-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2017047560-A1 |
priorityDate | 2001-09-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 137.