http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2005344048-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_5b354acbffbe119a27ccd31d99fdd8df |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L51-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L25-04 |
filingDate | 2004-06-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b746cc8ca347772d7422fc0df98f20d0 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_77c433b04df62113d8c198fec54347a0 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_213ec2f4ce2055b341456463b370d429 |
publicationDate | 2005-12-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2005344048-A |
titleOfInvention | Polystyrene modifier |
abstract | PROBLEM TO BE SOLVED: To provide a modifying material capable of greatly improving the weather resistance and thermal stability of a polystyrene resin. A (meth) acrylic acid ester unit is present in the presence of 5 to 60 parts by weight of an acrylic ester rubbery polymer having a gel content of 85% or more and a weight average particle size of 0.5 to 1.5 μm. Per 100 parts by weight of graft copolymer (A) obtained by copolymerizing 40 to 95 parts by weight of monomer (total) consisting of 10 to 30% by weight of monomer and 90 to 70% by weight of styrene monomer Polystyrene modifier with addition of 0.1 to 5 parts by weight of hindered amine light stabilizer and / or antioxidant and 0.01 to 1 part by weight of silicone oil [Selection] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2007176976-A |
priorityDate | 2004-06-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |