Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_28b36d00f47561309ac4f7c5944edafa |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-548 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-0025 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L9-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J3-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-5398 |
classificationIPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29K105-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29L30-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29K9-06 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C33-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B60C1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C35-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-47 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L9-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-5398 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-548 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K9-04 |
filingDate |
2005-05-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d442c75bf66e47c5e6fde34929e66f23 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5831f31dd924331e8408516b1b85cdc3 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b5c6277610ec5529626fc160b17d5f12 |
publicationDate |
2005-12-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2005336483-A |
titleOfInvention |
Process for producing a rubber mixture |
abstract |
[PROBLEMS] To provide a rubber composition suitable for producing NBR rubber having reversion stability suitable for producing a winter tire. A step of reacting one diene elastomer with at least one light-color reinforcing filler and at least one polysulfide-containing alkoxysilane, and one vulcanizing agent and at least one disulfide-containing alkoxysilane. A thiophosphate compound and at least one vulcanization accelerator selected from a sulfenamide compound and a thiazole compound are mixed. [Selection figure] None |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-4499658-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2007169559-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2016002506-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008106113-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2011122136-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9102812-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2007231065-A |
priorityDate |
2004-05-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |