http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2005329720-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_ad2cd796f8c4dcb425ddcc68707d3444 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29K67-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29L11-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29L7-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29L9-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B1-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B7-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C55-16 |
filingDate | 2005-06-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_75169bdd42220e74b25d121a768d1eeb http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b1c0e81b28f5081426e74252a64f69b3 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5fef018803b56d6c6a3401533509d3ca |
publicationDate | 2005-12-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2005329720-A |
titleOfInvention | Method for producing optical laminated film |
abstract | The present invention provides a method for producing an optical laminated film that is excellent in adhesiveness to other members and the like, has few optical defects, and is excellent in transparency. A method for producing a laminated film, comprising a biaxially oriented polyester film having a thickness of 50 μm or more as a base material, and forming an adhesive modified resin layer containing a resin and particles on at least one side of the base material. The material production process includes: (i) a process for producing an unstretched sheet made of polyester substantially containing no particles; (ii) a process for simultaneously biaxially stretching the unstretched sheet; and (iii) a film winding process. When manufacturing the base film, (a) a method that does not cause defects that cause scratches on the film surface or the roll surface that comes into contact with the film, (b) By using the method of preventing the displacement, the total scratches having a depth of 1 μm or more and a length of 3 mm or more existing on the surface of the laminated film are made 100 pieces / m 2 or less. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-102205634-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-102205634-B http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10550496-B2 |
priorityDate | 2000-12-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 188.