http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2005325193-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_24aca9ded2638ea793d05360dde7a4a0 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-00 |
filingDate | 2004-05-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_65404e4404d91323317f9dadbe0550a3 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_58b54eaba7e4f1be8e6a0ede89ac6c88 |
publicationDate | 2005-11-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2005325193-A |
titleOfInvention | Olefin resin composition and film comprising the resin composition |
abstract | PROBLEM TO BE SOLVED: To provide an olefin resin composition excellent in heat resistance, flexibility, and wide workability in air-cooled inflation molding, and a film comprising the resin composition. SOLUTION: An amorphous α-olefin copolymer 70 having a crystalline olefin polymer 30 to 80% by weight, a melt flow rate of 0.01 to 50 g / 10 minutes, and satisfying the formula (1). An olefin-based resin composition containing ˜20% by weight and a film comprising the resin composition. Ua ≦ 1.5 × Sa × (Ta / 100) 3.3 formula (1) (In Formula (1), Ua represents the flexural modulus of the evaluation resin composition comprising 50% by weight of the amorphous α-olefin copolymer and 50% by weight of the specific homopolypropylene, Sa represents the bending elastic modulus of the homopolypropylene resin contained in the resin composition for evaluation, Ta represents the blending ratio (50% by weight) of the homopolypropylene resin contained in the evaluation resin composition. ) [Selection figure] None |
priorityDate | 2004-05-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 136.