Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_aa67eb74ea5b96d9f8f2cfdb3b025770 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03B2205-57 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03B2205-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03B2201-22 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C25-6293 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C25-607 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C25-60 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C25-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03B37-02718 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03B37-027 |
classificationIPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B6-02 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03C25-60 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03B37-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B6-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03C25-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03B37-027 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03C25-62 |
filingDate |
2005-05-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_036a62012a2ea34f0a36b953fd7cce5a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f4b38f0b1ffa82052df973e3475909f8 |
publicationDate |
2005-11-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2005325019-A |
titleOfInvention |
Optical fiber manufacturing method |
abstract |
An object of the present invention is to solve the problem that the transmission characteristics of an optical fiber deteriorate due to the presence of hydrogen in the optical fiber. A method of manufacturing an optical fiber by contacting the optical fiber with deuterium, a deuterium-containing gas mixture or deuterium ion plasma during the stretching operation. The treatment or coating is performed in a treatment tube that is separated from or combined with the fiber cooling tube. [Selection figure] None |