http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2005324187-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_bb35bfe7ceb6ccdc2a0c9b447c0ffda8 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D7-24 |
filingDate | 2005-04-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_175c4a429bedd2f65193bed3c931a20a |
publicationDate | 2005-11-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2005324187-A |
titleOfInvention | Painting method |
abstract | An object of the present invention is to prevent a plasticizer in such a material from being transferred to a coating film by applying it to the surface of a sealing material or a vinyl interior material containing a plasticizer. Provided is a coating method capable of preventing the occurrence of cracks in a coating film caused by expansion and contraction of a system interior material or the like. An aqueous resin (I) having an average particle diameter of 0.1 μm or less and an elongation of a film of 500% or less on the surface of a material containing a plasticizer is 100 parts by weight in terms of solid content and average particles Organic powder (a) made of a polymer having a diameter of 0.1 to 100 μm and a glass transition temperature of −60 to 60 ° C. and / or an average particle diameter of 0.1 to 100 μm and a glass transition temperature of 30 ° C. An aqueous paint containing 3 to 400 parts by weight of an organic powder (II) made of an organic powder (b) having a core part made of less than a polymer and a shell part made of a polymer having a glass transition temperature of 30 ° C. or higher is applied. To do. [Selection figure] None |