Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_9592efd24c0c67b5f1b405d7d0c0c29a |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02A20-20 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/F16L9-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/F16L55-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J7-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/F16L11-12 |
filingDate |
2004-05-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6163531455f3e5d3de30e44a937e7c0b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2850a68f0422587bec97fe0875c050e9 |
publicationDate |
2005-11-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2005321028-A |
titleOfInvention |
Plastic piping members |
abstract |
PROBLEM TO BE SOLVED: To provide a resin piping member having weather resistance, antifogging property and antifouling property and capable of maintaining transparency over a long period of time. SOLUTION: A separator layer 3 and a photocatalyst layer 4 are laminated in order from the inside on the outer surface portion of a body 5 of a resin piping member (Y-type strainer). The separator layer 3 is formed with a coating solution containing amorphous titanium oxide with a film thickness of 1 μm by spray coating. The photocatalyst layer 4 is formed by coating a coating solution containing anatase-type titanium oxide with a film thickness of 0.1 μm by a spray coating method. [Selection] Figure 1 |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2013129585-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2013129586-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2009222131-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9463436-B2 |
priorityDate |
2004-05-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |