http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2005320661-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_8bcf612dd6863e11ef7d506d78193626 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D21H21-16 |
filingDate | 2004-05-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f27bd8b4f213ba100b71e051a591232d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_79b83b35d70807bd443ccf677b11c6da http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_606bd564ed3251be05519a75150a9f57 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_36e4e005d8db415dd3d24992111e05b5 |
publicationDate | 2005-11-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2005320661-A |
titleOfInvention | Newspaper for offset printing |
abstract | 【Task】 The problem to be solved by the present invention is to provide newsprint paper for offset printing that does not have any trouble during offset printing and has excellent offset printing workability. [Solution] The present invention relates to a newsprint for offset printing, which is obtained by applying a surface treatment agent comprising a water-soluble polymer substance as a main component and a surface sizing agent on a base paper for newsprint printing and then drying. A surface tension of 1% concentration of the surface treatment agent is set to 35 mN / m or less, and this is coated and dried to obtain newsprint paper for offset printing that is free from drip trouble and has excellent offset printing workability. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008248451-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2007070758-A |
priorityDate | 2004-05-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |