http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2005320487-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_b55c349b43c3ecba4977fd52cc8f8c67 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J133-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J7-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J157-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J201-00 |
filingDate | 2004-05-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1ce6094996fccbaf6a491da69cce28f2 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_246b16f6dac2bd0fad59e90670090291 |
publicationDate | 2005-11-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2005320487-A |
titleOfInvention | Manufacturing method of adhesive sheet |
abstract | PROBLEM TO BE SOLVED: To provide a method for producing a pressure-sensitive adhesive sheet that can obtain an extremely smooth coated surface and is suitably used for surface protection of an optical material. SOLUTION A surface at 25 ° C. obtained by a maximum bubble pressure method when a water-dispersed pressure-sensitive adhesive composition in which a base polymer composed of an acrylic polymer is dispersed in water is diluted with water to a solid content of 1% by weight. The tension is 25 mN / m or more and 50 mN / m or less when the bubble generation speed is 0.1 second / piece, and the tension is 25 mN / m or more and 43 mN / m or less when the bubble generation speed is 1 second / piece. The base material 1 is coated. In this method, it is possible to prevent the occurrence of coating stripes on the coated surface (the surface of the pressure-sensitive adhesive layer 2), and it is possible to form the pressure-sensitive adhesive layer 2 having high-precision smoothness. As a result, the obtained pressure-sensitive adhesive sheet can be suitably used for surface protection of an optical material for performing an appearance inspection of a product with the pressure-sensitive adhesive sheet adhered. [Selection] Figure 1 |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2016106168-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9181458-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-3878877-A1 |
priorityDate | 2004-05-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 181.