http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2005316142-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_cebc9740ef706cde29e885504f274ffa |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G9-087 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G9-08 |
filingDate | 2004-04-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6ff7cf9f88cbfe9e2dcc1a0db628e903 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8741444aaaf00829ba6fa5cb61bed0b5 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_80af6df637a54682c34373c6f747b088 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_44b8ccf22f35f2046a77a095165e43cf |
publicationDate | 2005-11-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2005316142-A |
titleOfInvention | Binder resin composition for pulverized toner, method for producing the same, and pulverized toner |
abstract | PROBLEM TO BE SOLVED: To provide a toner having an excellent balance between low-temperature fixability and non-offset property, a binder resin used therefor, and a method for producing the same. A styrene binder resin composition for a pulverized toner containing 0.5 to 25 parts by mass of a fatty acid ester having a melting point of 70 to 90 ° C. and a branched structure with respect to 100 parts by mass of a vinyl polymer, and This styrenic binder resin composition is obtained by polymerizing a vinyl monomer in the presence of the fatty acid ester, and this is used as a binder resin composition for a toner. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20170126957-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101971487-B1 |
priorityDate | 2004-04-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 84.