Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_b55c349b43c3ecba4977fd52cc8f8c67 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D7-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B5-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D3-02 |
filingDate |
2004-04-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d6450dd75c053cdf2d14aa912aa8d431 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_fb88a89949dfadfaeb9cebb5e29cc1e6 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_58aa70e8b22c150a98b63d82df8f3fab http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0dfed05062b3221dbaa49fb49497fbad http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_29ba9a1a947afbb0eb22c507383ea266 |
publicationDate |
2005-11-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2005313118-A |
titleOfInvention |
Coating film forming method, optical film and image display device |
abstract |
PROBLEM TO BE SOLVED: To form a uniform coating film relatively easily even for a base film having a large variation in surface free energy. SOLUTION: In a drying process of a coating film formed by applying a coating liquid on the surface of a base film having a variation in surface free energy of 2.5 mN / m or more, a drying temperature corresponding to the variation in surface free energy. To dry the coating film. The drying temperature to be set is a temperature determined so that the rate of change in thickness of the coating film is 5% or less. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101331713-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2015200831-A |
priorityDate |
2004-04-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |