http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2005306970-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_0a521cfa321c963978df8ae98a84056a |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L101-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-07 |
filingDate | 2004-04-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7fede75ce190948d381e6190a813cd2a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ecf818f5cc56bf6668d7eafeedb13a0c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1577fe03c36bb9ca3f53e1f4e4b02d71 |
publicationDate | 2005-11-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2005306970-A |
titleOfInvention | Method for curing thermosetting resin |
abstract | PROBLEM TO BE SOLVED: To suppress the generation of volatile organic chemical substances (VOC) such as formaldehyde at the time of curing while maintaining the curing characteristics of a thermosetting resin, and further reduce the residual amount of monomers such as styrene in a cured product. A method for curing a thermosetting resin is provided. [Solution] A method for curing a thermosetting resin, comprising adding 0.01 to 10 parts by weight of hydroperoxide and 0.05 to 5 parts by weight of acetylacetone with respect to 100 parts by weight of a thermosetting resin. Furthermore, the hardening method of the thermosetting resin which adds 0.01-10 weight part of acetoacetic acid derivatives with respect to 100 weight part of thermosetting resins. [Selection figure] None |