http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2005281508-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1150d1d80ff7a4912c50ba531a56d6f2 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09K11-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09K11-67 |
filingDate | 2004-03-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_13504914ce819aa86698540d9fd9d8c2 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b2f018fdd8c2f16f99050e8321c3515d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b8a7ab8c87f041f778afed69156e7108 |
publicationDate | 2005-10-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2005281508-A |
titleOfInvention | Method for manufacturing phosphor |
abstract | PROBLEM TO BE SOLVED: To provide a method for producing an oxide phosphor that has a longer life than a SrTiO 3 : Pr, Al phosphor and emits light with high brightness even with a low-speed electron beam. In a mixing step P1, a base material, a Pr source, a Li source, and the like are mixed, and in a firing step P4, the mixture is fired at a temperature within a range of 1050 to 1150 (° C.). Therefore, a CaTiO 3 : Pr, Li oxide that has a longer lifetime than a SrTiO 3 : Pr, Al phosphor and emits light with high brightness of 50 (cd / m 2 ) or more even when excited by a low-energy electron beam A phosphor is obtained. [Selection] Figure 1 |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2009242735-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8465676-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2009298997-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2015531412-A |
priorityDate | 2004-03-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |