http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2005264345-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_5d123e76a98aad8db100e9f8c62e0648 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D02G1-02 |
filingDate | 2004-03-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_53324fa9c426da61220d1e56b01ce1d8 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8c0ac0bd84f714539d83fe509548ee11 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b1f7cdc86b030f2688ed9fb2b3f89897 |
publicationDate | 2005-09-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2005264345-A |
titleOfInvention | Polyester false twisted yarn and method for producing the same |
abstract | PROBLEM TO BE SOLVED: To provide a polyester false twisted yarn excellent in gloss and a method for producing the same. For example, a polyester yarn having a birefringence (Δn) of 0.1 or more and a density (ρu) of 1.375 g / cm 3 or more, and a false twisted side tension of 0.25 to 0.45 cN / False twisting is performed under the condition of dtex to obtain a polyester false twisting yarn having a cross-sectional flatness coefficient (S) of 1.05 to 1.20 and a total crimp rate (TC) of 1.0 to 20%. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2010201811-A |
priorityDate | 2004-03-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 21.