http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2005254655-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_2d4d8115282cf75bb54e672fbbdb0576 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B41M5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B41J2-01 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B41M5-52 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B41M5-50 |
filingDate | 2004-03-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2d2a2d56534e45a7cb04d067967ed53b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e88c331d49d7c583fd806b52ba6f9a41 |
publicationDate | 2005-09-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2005254655-A |
titleOfInvention | Inkjet recording paper manufacturing method |
abstract | PROBLEM TO BE SOLVED: To provide a method for producing a photographic image quality inkjet recording paper having high ink absorbency without deteriorating productivity and fragility of a film. An aqueous coating solution containing inorganic fine particles and polyvinyl alcohol having a saponification degree of 90 mol% or more is coated and dried on a polyolefin-coated paper support in which both sides of the paper are coated with polyolefin, and a porous ink absorbing layer is formed. A method for producing an ink jet recording sheet, comprising: holding at least 10 seconds or more in a range of 70 to 95 ° C. after forming and then cooling to 40 ° C. or less and winding up into a roll. [Selection figure] None |