http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2005248174-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_6c8d4dc7bd1a30d8fda907fceaeb4e69 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-78 |
filingDate | 2005-02-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_031f5abd443342da1b12af7cc78b785e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_14dfb21a665c36d6815695d2f9d59cce http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a7d5bed8d14325adb4467b0cbc4ce667 |
publicationDate | 2005-09-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2005248174-A |
titleOfInvention | Heat exchanger cleaning method and polyester manufacturing method |
abstract | PROBLEM TO BE SOLVED: To provide a method for producing stable quality polyester and a heat exchanger cleaning method for achieving the method. In a process for producing a polyester by using 1,4-butanediol as a component and performing a polycondensation reaction in a molten state at a pressure of 10 kPa or less using a polymerization catalyst. A method for cleaning a condenser or a heat exchanger, wherein the condenser for condensing the condensed gas or the heat exchanger for cooling the condensed liquid of the distilled gas is washed at 50 to 300 ° C. [Selection] Figure 1 |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2007238496-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2009084443-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2009173884-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-2228399-A4 |
priorityDate | 2004-02-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 86.