http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2005220152-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_24aca9ded2638ea793d05360dde7a4a0 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F8-50 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J3-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F8-50 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F255-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F255-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F10-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F8-00 |
filingDate | 2004-02-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_bbeacd4719d512447c34d73e2b87be89 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_034e63e0c5bea1534de8ac9723720a79 |
publicationDate | 2005-08-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2005220152-A |
titleOfInvention | Process for producing modified polyolefin resin and modified polyolefin resin |
abstract | PROBLEM TO BE SOLVED: To provide a modified polyolefin resin having a lower molecular weight of a modified polyolefin resin to be produced as compared with a molecular weight of a polyolefin resin used as a raw material, a large amount of grafting, and excellent paintability, particularly in a water-based paint. A production method and a modified polyolefin resin produced by the method are provided. A method for producing a modified polyolefin resin, in which (B) 0.1 to 20 parts by weight and (C) 0.01 to 20 parts by weight are blended and melt-kneaded with respect to 100 parts by weight of the following (A). And the modified polyolefin resin manufactured by this method. (A) Polyolefin resin (B) Compound represented by the following structural formula (1) (C) Organic peroxide having a decomposition temperature of 50 to 115 ° C. when the half-life is 1 minute [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2020012973-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2020012974-A |
priorityDate | 2004-02-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 94.