http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2005165077-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_03d0f52bb4069f8a19d70dcfb697c67a |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C1-498 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C1-76 |
filingDate | 2003-12-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_77d0592288a3b52e157a1c227fbea5f9 |
publicationDate | 2005-06-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2005165077-A |
titleOfInvention | Photothermographic material |
abstract | PROBLEM TO BE SOLVED: To provide a photothermographic material excellent in storability of a back layer, particularly a photothermographic material in which devitrification of a back surface is suppressed. A photothermographic material having an image forming layer containing a photosensitive silver halide, a non-photosensitive organic silver salt, a reducing agent and a binder on one surface side of a support, wherein On the back surface side, which is the surface opposite to the surface having the image forming layer, has an antihalation layer containing a dye that is decolored by heat development, a base precursor, and a binder, and the binder of the antihalation layer is, A photothermographic material comprising an aqueous dispersion of a hydrophobic polymer in an amount of 60% by mass or more, and an application amount of the base precursor of 0.001 g / m 2 or more and 0.25 g / m 2 or less. [Selection figure] None |
priorityDate | 2003-12-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 378.