Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_d93502a23a72b56472bc75854cfe7c60 |
classificationIPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29K19-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29K105-24 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C35-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L71-03 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-092 |
filingDate |
2003-11-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_fed82d743292c3dc5dcd003b31082598 |
publicationDate |
2005-06-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2005154686-A |
titleOfInvention |
Epihalohydrin rubber composition |
abstract |
PROBLEM TO BE SOLVED: To provide an epihalohydrin rubber composition excellent in storage stability capable of giving a crosslinked molded article having a small compression set. SOLUTION: (A) 100 parts by weight of epihalohydrin rubber, (B) a crosslinking agent, (C) an acid acceptor, and (D) a chain saturated dicarboxylic acid having 3 to 20 carbon atoms, 0.2 to 2.0 parts by weight. An epihalohydrin rubber composition having a Mooney scorch time t5 retention of 50% or more. [Selection figure] None |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-102942779-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2007314588-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-101570630-B http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-102942779-B |
priorityDate |
2003-11-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |