http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2005149906-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_86ff778280a8f314c5732fead5868411 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02P70-50 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-05 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-0525 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-0587 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-505 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-485 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-02 |
filingDate | 2003-11-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_46ad9e1158fdc54ff5445a3f63d68ef8 |
publicationDate | 2005-06-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2005149906-A |
titleOfInvention | Cathode active material for nonaqueous electrolyte secondary battery, nonaqueous electrolyte secondary battery, and method for producing nonaqueous electrolyte secondary battery |
abstract | 【Task】 Provided are a positive electrode active material for a non-aqueous electrolyte secondary battery having excellent battery characteristics even in a more severe use environment, a non-aqueous electrolyte secondary battery, and a method for producing a non-aqueous electrolyte secondary battery. [Solution] A positive active material for a non-aqueous electrolyte secondary battery, a main active material having at least a first lithium transition metal composite oxide having a spinel structure, and a secondary active material having at least a second lithium transition metal composite oxide having a spinel structure A positive electrode active material for a non-aqueous electrolyte secondary battery, wherein the constituent elements of the main active material and the sub active material are the same, and the crystal structure of the second lithium transition metal composite oxide The lithium ion is present at the 16c site. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2016518687-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10741841-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8501353-B2 |
priorityDate | 2003-11-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 106.