Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_b55c349b43c3ecba4977fd52cc8f8c67 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-249946 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-249921 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T442-2992 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-24995 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J5-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02F1-1333 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J5-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02F1-133305 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K7-14 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K7-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B17-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L101-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G09F9-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02F1-1333 |
filingDate |
2004-07-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0b5eef32260b617902bd9765b6da6d42 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f1c82eae8915bd24bc11648345c29826 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1c3dbf24b9bf7098db0973a0184109f6 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6983ada5f460eba96100bfa81281f5c5 |
publicationDate |
2005-06-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2005146258-A |
titleOfInvention |
Optical resin sheet, liquid crystal cell substrate including the optical resin sheet, liquid crystal display device, image display device substrate, and image display device |
abstract |
PROBLEM TO BE SOLVED: To provide an optical resin sheet capable of improving display quality while having a low thermal expansion coefficient and excellent mechanical strength. The present invention comprises a cured resin layer containing glass fibers, and the ratio of the elastic modulus of the glass fibers to the elastic modulus of the cured resin constituting the cured resin layer is 25 or more. A resin sheet is provided. [Selection] Figure 1 |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2008044397-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2007010834-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8084131-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9249126-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2009058974-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2017221549-A1 |
priorityDate |
2003-10-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |