http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2005146015-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_68496d12a251010a470395787518f996 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F6-12 |
filingDate | 2003-11-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e677244a87020ad641c87e219049750e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_bbbacfe5101599865483ca897ebce533 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_031848646c1af956409944e4d631bf07 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0dd1cb62203ec40041b3a83cdfa7ea7c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_689d30f69e0e0e93b3ee7562567b2c22 |
publicationDate | 2005-06-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2005146015-A |
titleOfInvention | Solidification method of polypropylene or modified polypropylene |
abstract | Disclosed is a method for solidifying polypropylene or modified polypropylene, which reduces polymer loss and solvent loss and is excellent in productivity and economy. [Solution] 13 The racemic dyad fraction [r] measured by C-NMR is 0.12 to 0.88, the weight average molecular weight (Mw) is 5,000 to 500,000, and the solubility in toluene at room temperature is 5 g or more. A method of solidifying polypropylene from a polymer solution containing soluble polypropylene, wherein the solvent is removed from the polymer solution at 200 ° C. using any method selected from the group consisting of a film drying method, a steam distillation method, and a vacuum kneading method. The present invention provides a method for solidifying polypropylene, characterized by separating the polypropylene by vaporizing in the following. |
priorityDate | 2003-11-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 662.