http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2005132988-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_cebc9740ef706cde29e885504f274ffa |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L51-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L101-00 |
filingDate | 2003-10-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_20706c99b2899125189891d7718d20af http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4420546e2d8d94c23ba6dc2332ef8720 |
publicationDate | 2005-05-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2005132988-A |
titleOfInvention | Thermoplastic resin composition and molded article |
abstract | PROBLEM TO BE SOLVED: To provide a thermoplastic resin composition excellent in impact resistance, weather resistance and molding processability. The thermoplastic resin composition of the present invention is a composite rubber-like material containing polyorganosiloxane (S) and poly (meth) acrylate ester (M) containing a (meth) acrylate monomer unit. 1 to 99 parts by mass of a graft copolymer (A) in which a vinyl polymer is grafted to the polymer (R), and 99 to 1 part by mass of a vinyl copolymer (B) (provided that the graft copolymer ( A) and the vinyl copolymer (B) are 100 parts by mass.) And other thermoplastic resins (F) 0 to 80 parts by mass, and the graft copolymer (A) and It is characterized by further containing 0.1 to 10 parts by mass of polyalkylene glycol (C) with respect to 100 parts by mass in total of the vinyl copolymer (B) and the other thermoplastic resin (F). [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101432633-B1 |
priorityDate | 2003-10-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 93.