http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2005128054-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_67f2bb9a79bd8433343ae221f81551cf |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C1-76 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C1-74 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C1-498 |
filingDate | 2003-10-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_228315b7a9cbe04adfcd49fb8e9b4231 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b025e5db567230614be30a1553df5577 |
publicationDate | 2005-05-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2005128054-A |
titleOfInvention | Silver salt photothermographic dry imaging materials |
abstract | PROBLEM TO BE SOLVED: To provide a silver salt photothermographic dry imaging material having good coatability and excellent in-plane uniformity of a processed image. A silver salt photothermographic dry imaging material having an image forming layer on at least one surface of a support and at least one protective layer on the image forming layer, wherein at least one layer of the image forming layer is formed. A silver salt photothermographic dry imaging material obtained by applying and drying an image forming layer coating solution within the following viscosity conditions. (Viscosity condition): At 23 ° C., immediately after applying shear at a shear rate of 1000 (1 / s) for 30 seconds, the following equation is satisfied when vibration is applied for 5 minutes with a strain of 0.4 and a frequency of 2 Hz. 1.09> η B / η A > 1.02 However, η A : Viscosity immediately after starting vibration, η B : Viscosity 5 minutes after starting vibration [Selection] None |