http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2005121853-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_67f2bb9a79bd8433343ae221f81551cf http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_2d4d8115282cf75bb54e672fbbdb0576 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C7-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C1-74 |
filingDate | 2003-10-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_82fe5a5d6e10083211e476c897bc46b0 |
publicationDate | 2005-05-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2005121853-A |
titleOfInvention | Method for producing silver halide color photosensitive material |
abstract | PROBLEM TO BE SOLVED: To provide a method for producing a silver halide color light-sensitive material having a small change in fog density when a bleaching solution or a bleach-fixing solution is mixed in a color developing solution, and having excellent color reproducibility and color developing property. . A photosensitive layer containing at least one layer of gelatin, a photosensitive silver halide emulsion, and a dye-forming coupler represented by the following general formula (a) is coated on a support, followed by a drying step. The photosensitive layer is dried in a drying region where the moisture content (water content / gelatin mass × 100 (%)) is from 500% or less to the end of drying. A method for producing a silver halide color photographic material, characterized by being exposed to a drying zone (I) having a sphere temperature of 40 ° C. or more and 60 ° C. or less for 30 seconds or more and 120 seconds or less. [Chemical 1] [Selection figure] None |
priorityDate | 2003-10-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |