http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2005120260-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_7ef01e33058cf740cf2197991be97af1 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-87 |
filingDate | 2003-10-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_75fe3aaccf0dd64de4c51ed8ee491d71 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_929f46bfc6a0f363bb2ad09593741734 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_05d556e7e739bbf0002dabc9e39f5753 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b37ce0417ba0235694b0ead27389899f |
publicationDate | 2005-05-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2005120260-A |
titleOfInvention | Polyester resin and hollow molded body comprising the same |
abstract | 【Task】 To provide a polyester resin that generates less acetaldehyde during molding and hardly generates mold stains. [Solution] A polyester resin produced by polycondensation of an aromatic dicarboxylic acid and an aliphatic diol, which satisfies the following (a), (b), (c); (A) [Ti] / [P] ≧ 1 (In the formula, [Ti] represents the molar amount of titanium atoms contained in 1 ton of the polyester resin, and [P] represents the molar amount of phosphorus atoms contained in 1 ton of the polyester resin.) (B) ΔCT ≦ 0.1 (% by weight) ΔCT = [CT] 1 − [CT] 0 ([CT] 0 and [CT] 1 indicate the cyclic trimer content (% by weight) contained in the polyester before and after molding at 290 ° C., respectively.) (C) [CT] 0 ≦ 0.50 (wt%) |
priorityDate | 2003-10-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 113.