http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2005104992-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_bb4ee28d43b5e8d4a3c5141fa9bcfeb0 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F214-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F214-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F214-22 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F214-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L27-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F2-38 |
filingDate | 2003-07-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f78cb22a2a0df09be17add56c64fc82c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a281611fe9c11deea06e51480b177f7e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e2847469d64eca8ff131fe73cc1d253a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_22fe5ecbc43d5bba2f5956db6d46f872 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b9a989e95003e174a29b751e0aa93c61 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5f1ee5dd4bdb633b01a8dfba098529d4 |
publicationDate | 2005-04-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2005104992-A |
titleOfInvention | Method for producing vulcanizable fluorine-containing elastomer |
abstract | The present invention provides a method for producing a fluorine-containing elastomer having high productivity comparable to the non-iodine transfer polymerization method by performing iodine transfer polymerization under high pressure. Furthermore, the fluorine-containing elastomer obtained by this method and a fluorine-containing molded product are provided. A conversion temperature of a critical constant calculated by using the Peng-Robinson equation from the critical temperature, critical pressure, and composition ratio of each monomer in a gas phase portion in a reaction vessel is 0.95 or more, and the conversion pressure is A method for producing a fluorine-containing elastomer by batch copolymerization performed under a condition of 0.80 or more, General formula: Rf ยท Ix (Wherein, Rf is a saturated or unsaturated fluorohydrocarbon group or chlorofluorohydrocarbon group having 1 to 16 carbon atoms, x is the number of bonds of Rf, and is an integer of 1 or more and 4 or less. In the presence of at least one fluoroolefin is copolymerized. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2013177592-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2009057499-A1 |
priorityDate | 2003-01-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 202.