http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2005089580-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_7ef01e33058cf740cf2197991be97af1 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J3-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F2-44 |
filingDate | 2003-09-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_fd1b2098ac93106043fa1a9ddd1a26ab http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_fcc24292e00bfe8514d7e6d220007d56 |
publicationDate | 2005-04-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2005089580-A |
titleOfInvention | Method for improving fluidity of polymer powder |
abstract | [PROBLEMS] To improve the fluidity of a polymer powder such as polyolefin powder in a powder flow environment, to prevent heat spots from occurring during polymerization, and to provide excellent fluidity even in dead spaces in piping and various facilities where the polymer powder moves. To provide a method for improving the fluidity of a polymer powder that can be ensured and does not generate a polymer lump or sheet. A method for improving the fluidity of a polymerized powder, comprising a step of polymerizing a monomer or a step of storing the obtained polymerized powder, wherein a specific fluidity improver is supplied to a powder flow environment field. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2018076448-A |
priorityDate | 2003-09-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 258.